Titanium Ti-6Al-2Nb-1Ta-0.8Mo (Ti-621/0.8), as-rolled
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Close Analogs: 3 other heat treatments of this alloy are in Matweb.
Key Words: Ti-621/0.8; UNS R56210; Ti-6211
Material Notes: As-rolled from above Beta Transus. Alpha Alloy.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Compressive Yield Strength
- Compressive Modulus
- Poissons Ratio
- Charpy Impact
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|