Titanium Ti-3Al-2.5V, ST 925°C, Aged 480°C
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Close Analogs: 3 other heat treatments of this alloy are in Matweb.
Key Words: Ti3Al2.5V, ST 925ºC, Aged 480ºC; Ti-3-2.5 STA; UNS R56320; ASTM Grade 9; Half 6-4; Tubing Alloy
Material Notes: Information provided by Allvac and the references. Applications: Excellent cold formability, 20-50% higher tensile properties than CP titanium grades. Primarily used in aircraft hydraulic systems.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|