Titanium Ti-6Al-2Nb-1Ta-1Mo, Annealed
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Close Analogs: 1 other heat treatment of this alloy is in Matweb.
Key Words: Ti6Al2Nb1Ta1Mo, Ti-6211; Ti-621/0.8; UNS R56210
Material Notes: Annealed 700-870°C for 15 - 120 min.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Notched Tensile Strength
- Poissons Ratio
- Charpy Impact
- Fatigue Strength
- Fracture Toughness
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|