Titanium IMI 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.25Si), Oil-Quenched and Aged
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Key Words: Ti11Sn5Zr2.25Al1Mo0.25Si
Material Notes: Alpha Prime Transus 880ºC. Tensile Properties below after oil quench/aged heat treatment: 900°C/OQ, 500°C/24hr/AC.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Poissons Ratio
- Fatigue Strength
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Beta Transus
|
|
|
|