Titanium Ti-5-5-2-3 (Ti-5Mo-5V-2Cr-3Al), 60 mm Bar, Aged
Subcategory: Titanium Alloy; Nonferrous Metal; Beta Titanium Alloy
Material Notes: Relative to Ti-10V-2Fe-3Al. Characterized by cold formable and weldable high strength Ti alloy, in high area reduction and high fracture toughness KIC. Applications: - Bars for deep well strings in the petroleum industry
- Rods diameter 8-20 mm for high strength bolts
- Near net shape forging application
- Thick wall vessel
- Ultra high velocity centrifugal rotor
Information provided by MarkeTech International.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Fracture Toughness
|
|
|
|