Titanium Transage 129, Solution Treated 760°C
Subcategory: Titanium Alloy; Nonferrous Metal; Beta Titanium Alloy
Close Analogs: See other heat treatments for this alloy as well as entries for Transage 134 and 175.
Key Words: Ti-11.5V-2Al-2Sn-11Zr; T129
Material Notes: This alloy has very good fatigue resistance, which is enhanced by an alpha-beta anneal at 650ºC before aging at 425-540ºC.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Beta Transus
|
|
|
|