Titanium Ti-13V-11Cr-3Al; (Ti-13-11-3) Annealed 800°C, 30 min.
Subcategory: Titanium Alloy; Nonferrous Metal; Beta Titanium Alloy
Close Analogs: 5 other heat treatments of this alloy are in MatWeb.
Key Words: Ti-13-11-3; B120VCA; UNS R58010
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Notched Tensile Strength
- Ultimate Bearing Strength
- Bearing Yield Strength
- Poissons Ratio
- Charpy Impact
- Fatigue Strength
- Fracture Toughness
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|