Titanium Ti-13V-2.7Al-7Sn-2Zr, ST 815°C, Aged 510°C
Subcategory: Titanium Alloy; Nonferrous Metal; Beta Titanium Alloy
Close Analogs: 5 other heat treatments of this alloy are in MatWeb.
Key Words: Transage 175
Material Notes: ST=solution Treated
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Poissons Ratio
- Fatigue Strength
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Beta Transus
|
|
|
|