Titanium Ti-15Mo-5Zr-3Al Duplex Aged
Subcategory: Titanium Alloy; Nonferrous Metal; Beta Titanium Alloy
Close Analogs: 5 other heat treatments of this alloy are in MatWeb.
Material Notes: Heat Treatment: Solution treated 735ºC, Aged 425ºC 16 h, Aged 500ºC 16 h. Beta Transus 785ºC
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Beta Transus
|
|
|
|