Titanium Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti-17) Alpha-Beta Processed
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Close Analogs: 1 other heat treatment of this alloy is in Matweb.
Key Words: UNS R58650
Material Notes: Information provided by Allvac and the references. Beta Transus 890ºC ; Alpha-Beta Alloy; Double Solution Treated 860ºC, 2h; 800ºC, 4h; Aged 620ºC, 8h. Applications: Compressor discs, heavy section forgings for gas turbine engine components. High tensile strength and good fracture toughness.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Notched Tensile Strength
- Poissons Ratio
- Fatigue Strength
- Fracture Toughness
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|