Titanium Ti-6Al-2Sn-2Zr-2Mo-2Cr-.25Si, Annealed
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Close Analogs: 3 other heat treatments of this alloy are in MatWeb.
Key Words: Ti-6-22-22-S
Material Notes: Alpha-Beta Alloy. Welding is not recommended.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Beta Transus
|
|
|
|