Titanium Ti-4Al-4Mo-2Sn-0.5Si (IMI550), STA
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Material Notes: Solution Treated 900ºC, Aged 500ºC. Alpha-Beta Alloy
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Notched Tensile Strength
- Poissons Ratio
- Charpy Impact
- Fatigue Strength
- Fracture Toughness
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Beta Transus
|
|
|
|