Titanium Ti-6Al-4V (Grade 5), ELI, Annealed
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Close Analogs: 4 other heat treatments of this alloy are listed in MatWeb.
Key Words: Ti-6-4; UNS R56400; ASTM Grade 5 titanium; UNS R56401 (ELI); Ti6Al4V, biomaterials, biomedical implants, biocompatibility
Material Notes: Information provided by Allvac and the references. Annealing Temperature 700-785ºC. ELI (Extra Low Interstitial) grade has lower impurity limits, especially oxygen and iron. Alpha-Beta Alloy Applications: Applications requiring excellent fracture toughness and fatigue strength; aircraft, structural components, biomedical.. Biomedical implants. Biocompatibility: Excellent, especially when direct contact with tissue or bone is required. Ti-6Al-4V's poor shear strength makes it undesirable for bone screws or plates. It also has poor surface wear properties and tends to seize when in sliding contact with itself and other metals. Surface treatments such as nitriding and oxidizing can improve the surface wear properties.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Compressive Yield Strength
- Notched Tensile Strength
- Ultimate Bearing Strength
- Bearing Yield Strength
- Poissons Ratio
- Charpy Impact
- Fatigue Strength
- Fracture Toughness
- Shear Modulus
- Shear Strength
- Electrical Resistivity
- Magnetic Permeability
- Magnetic Susceptibility
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|