Titanium Ti-6Al-4V (Grade 5), STA Bar
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Close Analogs: 4 other heat treatments of this alloy are listed in MatWeb.
Key Words: Ti-6-4; UNS R56400; ASTM Grade 5 titanium; UNS R56401 (ELI); Ti6Al4V, biomaterials, biomedical implants, biocompatibility
Material Notes: Information provided by Allvac and the references. Solution Treated 900-955ºC, Aged 540ºC. Alpha-Beta Alloy Applications: Blades, discs, rings, airframe, fasteners, components. Vessels, cases, hubs, forgings.. Biomedical implants. Biocompatibility: Excellent, especially when direct contact with tissue or bone is required. Ti-6Al-4V's poor shear strength makes it undesirable for bone screws or plates. It also has poor surface wear properties and tends to seize when in sliding contact with itself and other metals. Surface treatments such as nitriding and oxidizing can improve the surface wear properties.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Compressive Yield Strength
- Poissons Ratio
- Fatigue Strength
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- Magnetic Susceptibility
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|