AISI A6, Type Tool Steel, austenitized 830-870°C (1525-1600°F)
Subcategory: Tool Steel; Air-Hardening Steel; Cold Work Steel; Metal
Key Words: UNS T30106, ASTM A681, FED QQ-T-570
Material Notes: High hardenability, high dimensional stability in heat treatment. Good wear resistance, fatigue life, and toughness.
| Available Properties |
- Density
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|