AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C
Subcategory: Tool Steel; Cold Work Steel; High Carbon Steel; Metal
Close Analogs: AISI Type D3, AISI Type D4, AISI Type D5, AISI Type D7
Key Words: high carbon, high chromium, UNS T30402, ASTM A681, FED QQ-T-570, SAE J437, SAE J438, DIN 1.2379, B
Material Notes: High-carbon, High-chromium Tool Steel. Virtually non-deforming during heat treatment. High wear resistance, which increases with increasing C and V content.
| Available Properties |
- Density
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Izod Impact Unnotched
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|