Titanium Grade 3, Annealed
Subcategory: Titanium Alloy; Nonferrous Metal; Unalloyed/Modified Titanium
Close Analogs: Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.
Key Words: ASTM Grade 3; UNS R50550, CP titanium, C.P. titanium alloy
Material Notes: Information provided by Allvac and the references. Applications: Airframe skin, heat exchangers, cryogenic vessels, components for CPI equipment, condenser tubing, exhaust pipe shrouds. Sample was annealed 2 hr at 700°C.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Notched Tensile Strength
- Ultimate Bearing Strength
- Bearing Yield Strength
- Poissons Ratio
- Charpy Impact
- Fatigue Strength
- Shear Modulus
- Electrical Resistivity
- Heat of Fusion
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Liquidus
- Beta Transus
- Emissivity (0-1)
- Reflection Coefficient, Visible (0-1)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|