UNS F33100 Cast Iron
Subcategory: Metal
Key Words: 65-45-12, SAE J434 D4512
Material Notes: Iron content is calculated as a remainder.
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Compressive Yield Strength
|
|
|
|
| Property Data |