AMS 5315D(94) Ductile Iron
Subcategory: Ductile Iron; Metal
Key Words: 5315
Material Notes: Iron content is calculated as a remainder. This specification is obsolete.
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|