ASTM A874 Ductile Iron Composition
Subcategory: Ductile Iron; Metal
Key Words: ASTM A874M
Material Notes: C + 1/3 Si <= 4.5 wt.%. Ferritic microstructure, suitable for low temperature service.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|