W-5 Re Tungsten Rhenium Alloy, Annealed
Subcategory: Tungsten Alloy; Nonferrous Metal; Refractory Metal
Material Notes: Annealed applies only to tensile; other property values are typical of this alloy. Ductile to brittle transition temperature (DBBT) reports range -23 to 227°C. Recrystallization Temperature reports range 1200-1500°C (incipient) or 1500-1577°C (complete). Bcc crystal lattice. Information provided by Rhenium Alloys Inc.
| Available Properties |
- Density
- Modulus of Elasticity
- Poissons Ratio
- Melting Point
|
|
|
|