W-25 Re Tungsten Rhenium Alloy, Deformed
Subcategory: Tungsten Alloy; Nonferrous Metal; Refractory Metal
Material Notes: Deformed applies only to tensile; other property values are typical of this alloy. Ductile to brittle transition temperature (DBBT) (-100) - (25) °C. Stress relieving temperature 1200-1400°C. Recrystallization Temperature 1500-1650°C. Bcc crystal lattice. Information provided by Rhenium Alloys Inc.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Critical Superconducting Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Melting Point
|
|
|
|