Composition Spec for Aluminum A305.2
Subcategory: Aluminum Alloy; Nonferrous Metal; Aluminum Casting Alloy
Key Words: Aluminium A305.2
Material Notes:
The sum of 'Other' metallic elements 0.010 percent or more each, expressed to the second decimal before determining the sum. The aluminum content for unalloyed aluminum not made by a refining process is the difference between 100.00 percent and the sum of all other metallic elements present in amounts of 0.010 percent or more each, expressed to the second decimal before determining the sum. Includes listed elements for which no specific limit is shown. This database entry lists the complete composition spec as collected by TheMetalMarket. Other database entries have complete physical property data for most aluminum alloys.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|