Zinc Zn-Cu-Ti Alloy (Zn-0.8Cu-0.15Ti), Hot-Rolled
Subcategory: Zinc Alloy; Nonferrous Metal
Close Analogs: Properties vary with rolling direction. Values for longitudinal and transverse directions are listed separately.
Key Words: UNS Z41320
Material Notes: Hot Work Temperature 150-300°C
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fatigue Strength
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |