Rolled Zinc Alloy (Zn-1.0Cu-0.010Mg), Hot-Rolled - Transverse Properties
Subcategory: Zinc Alloy; Nonferrous Metal
Close Analogs: Properties vary with rolling direction. Average values and values for longitudinal direction are listed separately.
Key Words: UNS Z45330
Material Notes: Hot Work Temperature 175-300°C
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Vickers
- Tensile Strength, Ultimate
- Elongation at Break
- Fatigue Strength
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Annealing Temperature
- Hot-Working Temperature
|
|
|
|
| Property Data |