Zinc Slush Casting Alloy A (Zn-4.75Al-0.25Cu)
Subcategory: Zinc Alloy; Nonferrous Metal
Key Words: ASTM B792; UNS Z34510
Material Notes: Properties are for chill cast samples.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Elongation at Break
- Charpy Impact, Unnotched
- Melting Point
- Solidus
- Liquidus
|
|
|
|