Zinc AC41A Alloy, As Cast
Subcategory: Zinc Alloy; Nonferrous Metal
Key Words: ASTM C41A; SAE 925; UNS Z35530 (ingot), UNS Z35531 (casting); ASTM B240; ASTM B86, Mazak 5, Zamak 5, Zamac 5
Material Notes: The composition listed above is according to ASTM B86 specifications. Conflicting sources on composition. One source gives Mg content as 0.020 - 0.05% with a footnote saying the Mg content can be as low as 0.015% as long as the Pb, Cd, and Sn contents do not exceed 0.003, 0.003, and 0.001% respectively. The same source does not list Cu as a constituent of AC41A. Another source lists the Mg content as 0.030 - 0.080%. Suggested Casting Temperature 395-425°C (745-795°F).
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Elongation at Break
- Compressive Strength
- Charpy Impact, Unnotched
- Fatigue Strength
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Casting Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|