Latitude Manufactuing Technologies PowderFlo® 17-4PH Stainless Steel Metal Injection Molding Compound
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal
Close Analogs: Composition Notes: Iron content calculated as balance.
Key Words: PM, Powder Metallurgy, Metal Powder MIM, 17-4 PH Stainless Steel
Material Notes: Aqueous Agar Binder, Improved Gel Strength. Sintered properties are dependant on sintering conditions and specific parts. Sintered density > 98.5% is typical. Metal injection molding (MIM) allows metal parts to be produced using standard injection molding machinery. This manufacturing process allows intricate metal parts to be produced that either can not be produced or are cost prohibitive to produce using other metal fabrication processes. PowderFlo® MIM Compounds feature a patented aqueous agar-based binder system that is quickly and easily debound through simple air drying, offering an environmentally friendly production process. PowderFlo® MIM Compounds unique binder system also decreases limitations on part size and wall thickness that constrain the use of other MIM materials. PowderFlo® is a registered trademark of Latitude Manufacturing Technologies. Information provided by Latitude Manufactuing Technologies.
| Available Properties |
- Bulk Density
- Viscosity
- Linear Mold Shrinkage
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Feed Temperature
- Mold Temperature
- Moisture Content
- Injection Pressure
- Sintering Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|