AK Steel Hot Rolled Carbon Steel, Drawing Steel (DS Type B), Standard Grade
Subcategory: Carbon Steel; Low Carbon Steel; Metal
Material Notes: DS is made by adding aluminum to the molten steel and may be used in drawing applications.Information provided by AK Steel
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- Specific Heat Capacity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|