AK Steel Hot Rolled Carbon Steel, Medium/High Strength Low Alloy (HSLA), ASTM A 607 Class 2 Formable, Grade 45K
Subcategory: Carbon Steel; Low Carbon Steel; Metal
Material Notes: ASTM A 607 is for Hot Rolled and Cold Rolled grades. AK Steel produces Type 1 (columbium bearing only), Class 2 limits only C and has a 10 ksi difference between the minimum specified YS and UTS. AK Steel Formable Grade - K indicates killed.Information provided by AK Steel
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |