AK Steel ZINCGRIP® ELECTRASMOOTH Electrogalvanized Carbon Steel, High Strength Low Alloy Steel (HSLAS), FORMABLE 50K / ASTM A 607 Type 1 / SAE J1392 050 XLK, Grade 50
Subcategory: Carbon Steel; Low Carbon Steel; Metal
Material Notes:
Information provided by AK Steel
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|