AK Steel Aluminized Carbon Steel, Extra Deep Drawing Steel Plus (EDDS+), Standard Grade
Subcategory: Carbon Steel; Low Carbon Steel; Metal
Material Notes: Aluminized Type 1 coating contains approximately 91% aluminum and 9% silicon that is metallurgically bonded to the low-carbon steel substrate. Interstitial Free (I-F) steels are made by adding titanium and/or columbium to the molten steel after vacuum degassing and offer excellent drawability.Information provided by AK Steel
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Modulus of Elasticity at Elevated Temperature
- Maximum Service Temperature, Air
- Deep-Drawing Capability rm
- Strain Hardening Exponent n
|
|
|
|