AK Steel Enameling Carbon Steels, ASTM A 424 Type 1, UNIVIT DS
Subcategory: Carbon Steel; Low Carbon Steel; Metal
Close Analogs: Iron content calculated as remainder
Material Notes: UNVIT is a specialty enameling steel developed for applications where direct-on cover coat enameling is employed. This product is free of porcelain enamel fishscale regardless of the enameling system employed.Information provided by AK Steel
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Deep-Drawing Capability rm
- Strain Hardening Exponent n
|
|
|
|