AK Steel Ferritic Stainless steel 18 SR™
Subcategory: Stainless Steel; Metal; Ferritic
Close Analogs: Iron content calculated as remainder
Material Notes: AK Steel 18 SR™ provides excellent resistance to high temperature scaling - far superior to that of Type 446 stainless steel. This material is readily welded by conventional methods. It is not subject to troublesome embrittlement or loss of corrosion resistance in the heat affected zones that affects many other straight chromium alloys. Typical uses include industrial ovens, blowers, exhaust systems, furnace equipment, heaters, induction furnaces and furnace tubes, annealing boxes, baffle plates, heat exchangers, resistor grids, kiln liners and pyrometer tubes.Information provided by AK Steel
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Electrical Resistivity
- Maximum Service Temperature, Air
- Corrosion Resistance
- Deep-Drawing Capability rm
- Strain Hardening Exponent n
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|