AK Steel Ferritic Stainless steel 409Ni
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal; Ferritic
Close Analogs: Iron content calculated as remainder
Material Notes: AK Steel 409Ni is a nominal 11% chromium stainless steel micro-alloyed with titanium, manganese and nickel that provides excellent weldability, toughness and fabricating characteristics. AK Steel 409Ni is an ideal material for applications requiring weldability and toughness superior to standard Type 409, at relatively low cost.Information provided by AK Steel
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|