AK Steel Ferritic Stainless steel 434
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal; Ferritic
Close Analogs: Iron content calculated as remainder
Material Notes: AK Steel 434 is a modification of Type 430, the addition of molybdenum increases this alloy`s corrosion resistance and its attack from many deicing chemicals. It also provides good heat and oxidation resistance up to 1500°F as well as good mechanical properties. AK Steel 434 is Ferro-magnetic.Information provided by AK Steel
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|