AK Steel Ferritic Stainless steel 41003
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal; Ferritic
Close Analogs: Iron content calculated as remainder
Material Notes: AK Steel 41003 is an economical steel that provides excellent weldability, toughness and fabricating characteristics. This alloy is an excellent choice for applications such as tubing and sheet for bus frames, coal hopper cars, street sweepers, chutes, storage tanks, ISO shipping container frames and other equipment requiring low life-cycle costs.Information provided by AK Steel
| Available Properties |
- Hardness, Rockwell B
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
|
|
|
|