AK Steel Martensitic Stainless Steel 410
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal; Martensitic
Close Analogs: Iron content calculated as remainder
Material Notes: AK Steel 410 provides good corrosion resistance plus high strength and hardness. It is magnetic in both annealed and hardened conditions. A wide range of properties can be developed with different heat treatments. Applications requiring moderate corrosion resistance and high mechanical properties are ideal for this alloy. Typical uses include flat springs, knives, kitchen utensils and hand tools.Information provided by AK Steel
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fatigue Strength
- Electrical Resistivity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|