AK Steel Martensitic Stainless Steel 410 Cb
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal; Martensitic
Close Analogs: Iron content calculated as remainder
Material Notes: AK Steel 410 Cb is an improved version of standard Type 410. The addition of columbium offers 3 major advantages: 1) Greater ease in heat treating, 2) Higher strength and toughness, 3) Improved grain size control.Information provided by AK Steel
| Available Properties |
- Density
- Hardness, Rockwell B
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Charpy Impact
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity at Elevated Temperature
|
|
|
|