AK Steel Austenitic Stainless Steel 301

 

Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal; Austenitic

Close Analogs: Iron content calculated as remainder

Material Notes:
AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be achieved by rolling with lower loss of ductility. AK Steel 301 is non-magnetic when annealed, but becomes slightly more magnetic than other standard austenitic stainless steels when cold worked. Typical uses include aircraft structural parts, trailer bodies, diaphragms, utensils, architectural and automotive trim, automobile wheel covers, roof drainage products, table wear, and conveyor belts.

Information provided by AK Steel

Available Properties
  • Density
  • Hardness, Rockwell B
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • Magnetic Permeability
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity at Elevated Temperature
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。