AK Steel Austenitic Stainless Steel 304L
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal; Austenitic
Close Analogs: Iron content calculated as remainder
Material Notes: AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive conditions. It often eliminates the necessity of annealing weldments except for applications specifying stress relief. It has slightly lower mechanical properties than Type 304.Information provided by AK Steel
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity at Elevated Temperature
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|