AK Steel Precipitation Hardening Stainless Steel 15-5 PH, Condition H 900
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal; Martensitic
Close Analogs: Iron content calculated as remainder
Material Notes: AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, low-temperature heat treatments minimize distortion and scaling. AK Steel 15-5 PH® is the ferrite-free version of AK Steel 17-4 PH® Stainless Steel. Both alloys are widely used in the aerospace, chemical, petrochemical, food processing, paper and general metalworking industries. The material supplied from the mill is in Condition A. After fabrication eight standard heat treatments have been developed to provide a wide range of properties.Information provided by AK Steel
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- CTE, linear 20°C
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|