Excalibar® 6013-T651 Aluminum
Subcategory: Aluminum Alloy; Nonferrous Metal; 6000 Series Aluminum Alloy
Key Words: Aluminum 6013-T651; 6013-T651 Aluminium; Alcoa, Aluminum Company of America; A6013-T651; UNS A96013
Material Notes: Weldability = A; Stress Corrosion Cracking Resistance = A; General Corrosion Resistance = B (A = best; E = worst). General 6013 characteristics and uses: High strength and good corrosion resistance. Easily joined by all welding and brazing methods. Excellent compressive properties. Good applied coating acceptance and good machinability. Uses: ABS Braking systems, hydraulic applications, valves, machine parts, roller blade parts, munitions. Data supplied by the manufacturer, Alcoa.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Machinability
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|