Toolrite 2011®-T8 Aluminum
Subcategory: Aluminum Alloy; Nonferrous Metal; 2000 Series Aluminum Alloy
Key Words: 2011-T8 Aluminium; UNS A92011; Alcoa, Aluminum Company of America; AA2011-T8
Material Notes: Weldability = D; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting qualities, good mechanical properties. Excellent surface finish capability. The T451 temper offers good deep drilling characteristics. Uses: Adapters, carburetor parts, clock parts and gears, knobs, camera parts, meter shafts and gears, nozzles, pencil and pen parts, oil line filters, pipe stems and filters, radio parts, screwdriver caps, spindles, telephone parts, TV fittings, tripod fittings, machine parts, hose parts, pipe stems. Data supplied by the manufacturer, Alcoa.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Knoop
- Hardness, Rockwell A
- Hardness, Rockwell B
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fatigue Strength
- Machinability
- Shear Strength
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|