Alcoa Aluminum 2324-T39 Plate
Subcategory: Aluminum Alloy; Nonferrous Metal; 2000 Series Aluminum Alloy
Close Analogs: Aluminum content calculated as remainder
Key Words: Aluminium
Material Notes: Alloy 2324-T39 is a higher strength version of alloy 2024-T351 and is a purity controlled composition varient of alloy 2024. It was developed for tension-dominated, fatigue and fracture critical plate applications. The T39 temper, developed through special fabricating practices, improves both strength and fracture toughness properties over alloy 2024 plate. Alloy 2324-T39 plate is being used successfully on lower wing skin and center wing box components of new commercial transport aircraft. Information provided by Alcoa.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 68°F
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|