ALIMEX ACP 5080R Aluminum Cast Material
Subcategory: Aluminum Alloy; Aluminum Casting Alloy; 5000 Series Aluminum Alloy
Close Analogs: Homogenized and stress relieved
Key Words: AA 5083 (AlMg4.5Mn0.7) according to DIN EN 573-3
Material Notes: Extraordinary sizes range availability along with superior mechanical and physical properties of ACP 5080R provide the Mold Tool Industry tooling materials solutions for the most challenging applications.Information provided by ALIMEX GmbH
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 68°F
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|