ALIMEX ACP 6000 Aluminum Cast Plate
Subcategory: Aluminum Alloy; Aluminum Casting Alloy; 7000 Series Aluminum Alloy
Close Analogs: Homogenized and stress relieved
Key Words: Al-Alloy type 7xxx
Material Notes: Aluminum cast plate ACP 6000 is a 7xxx series alloy surface-machined plate. This type of alloy ensures excellent machinability characteristics and adequate tensile strength. Thickness, flatness and surface finish offer very close tolerances.Information provided by ALIMEX GmbH
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 68°F
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|