ALIMEX AMP 8000 Aluminum Plate
Subcategory: Aluminum Alloy; 7000 Series Aluminum Alloy
Key Words: Aluminium alloy
Material Notes: AMP 8000 offers higher strength levels, good machinability and dimensional stability. Its tensile strength is up to 40% higher than AlZn5.5MgCu (7075). Moulding, (Prototypes) injection moulds, Jig and fixture manufacturing, Tool manufacturing, Special machine construction, Standard parts.Information provided by ALIMEX GmbH
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 68°F
- Thermal Conductivity
- Machinability
- Polishing Properties
- Protective Anodising
- Welding Properties (WIG, MIG)
|
|
|
|