Nickelvac® 901 Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
Subcategory: Superalloy; Nickel Base
Key Words: Allvac, an Allegheny Teledyne Company, UNS N09901; AMS 5660, 5661
Material Notes: Iron content calculated as remainder. Data provided by Allvac. Applications: Turbine discs and shafts, compressor blades and discs, high-temperature bolting, high-temperature devices, cryogenics.