Nickelvac® H-N Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal
Subcategory: Superalloy; Nickel Base
Key Words: Allvac, an Allegheny Teledyne Company, UNS N10003; AMS 5771. ASTM B 434, B 573
Material Notes: Nickel content calculated as remainder. Data provided by Allvac. Applications: Turbine gas sealing components.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
|
|
|
|